Looks like you are not TradeKey.com's Member yet. Signup now to connect with over 11 Million Importers & Exporters globally. Join Now |
BOOK A CALL
Book Call On Your Favorite Time
Code
🗘

By Signing Up. I agree to TradeKey.com Terms of Use, Privacy Policy, IPR and receive emails related to our services

Contact Us
Sell Sodium Diethylhexyl Sulfosuccinate

Sell Sodium Diethylhexyl Sulfosuccinate

FOB Price

Get Latest Price

|

Minimum Order

Place of Origin:

CHINA

Price for Minimum Order:

-

Minimum Order Quantity:

10 Ton

Packaging Detail:

Package: 200L plastic drum, IBC(1000L), customersâ�ï¿&fr

Delivery Time:

two weeks

Supplying Ability:

3000 Ton per Month

Payment Type:

T/T, L/C

Contact Now
Free Member

Contact Person Mr. Guangtao

205Room, No15 Zhongtian Street, Downtown Zaozhuang city,Shandong Province,China, Zaozhuang, Shandong

Contact Now

Description

Properties:

This product is an anionic surfactant, it has properties of rapid penetration, homogeneity, wetting, emulsification and better frothing. It is intolerant with strong acid, strong alkali, heavy metals and reductant.

This product is soluble in water, lower alcohol, benzene, ccl4 and kerosene oil solvents. The solution is milk white, pH (1% water solution) is 6.5±0.5.

This product can penetrate rapidly and homogeneously, and has good effect at temperature lower than *0℃ and pH ***0. The treated fabric is stable even temperature acidic and alklic condition changed. It’s widely used textile & dyeing, pesticide emulsification, tanning and mineral separation.

Specification:
Items Index
Appearance Colorless or yellowish liquid
pH (1% water solution) 6.5±0.5
Penetrating(1% water solution) ≤5s
Solid content % *0±2
Methods and used in

(1) Cotton wool dyeing: 2g/l of this product is heated from room temperature to *5℃, *0 min dehydration, then rolling drift after cooling, cleaning, dechloridation.

(2) Cotton wool lian drift: cotton wool is pretreated at *0℃ for 5 min, then other additives can be added, it is heated to ****0℃ in ****0 min, and is treated for *5 min. When cotton shell is removed, it can be dyed. The preferred dosage is **3g/l.

(3) Cotton wool lian, drift and dyeing: The direct or active dye which is oxidant tolerance is selected. The method is the same as 2, dyeing is added directly.

(4) Scouring of adhesive: addition of penetrant t in scouring of adhesive can reduce 2 h and decrease damage to silk.

(5) Usage in asbestos: for froth asbestos, the preferred dosage is ****5% of asbestos; for dustless asbestos, the preferred dosage is ****0% of asbestos.

(6) Usage in tanning: for dry tanning, this product is usually mixed with jfc, and the preferred dosage is 0.**1.0%. For tanning additives, the preferred dosage is *0%.

Send a direct inquiry to this supplier

To:

Mr. Guangtao < Zaozhuang Youbang Chemicals Co., Ltd >

I want to know: